材質(zhì) | 化學(xué)成份 Chemical Composition (%) | 最高工作溫度 MAX WORK TEMP | 特 性 | |||||
C | Si | Mn | Ni | Cr | Mo | |||
A3 | ≤0.22 | ≤0.3 | ≤0.65 | - | - | - | 400° | 普通網(wǎng)帶 |
45# | ≤0.50 | ≤0.37 | ≤0.80 | ≤0.25 | ≤0.25 | - | 500° | 普通網(wǎng)帶 |
1cr13 | ≤0.15 | ≤0.6 | ≤0.6 | - | 12-14 | - | 650 ° | 普通網(wǎng)帶 |
1cr17 | ≤0.15 | ≤0.6 | ≤0.6 | - | 12-18 | - | 650 ° | 普通網(wǎng)帶 |
304M | ≤0.06 | ≤1.0 | ≤2.0 | 8.9-10.0 | 18-20 | - | 750° | 普通網(wǎng)帶 |
304L | ≤0.03 | ≤1.0 | ≤2.0 | 9-13 | 18-20 | - | 750° | 耐晶界腐蝕 |
316 | ≤0.08 | ≤1.0 | ≤2.0 | 10-14 | 16-18 | 2-3 | 750° | 耐腐蝕 |
316L | ≤0.03 | ≤1.0 | ≤2.0 | 12-15 | 16-18 | 2-3 | 750° | 耐晶界腐蝕 |
309S | ≤0.08 | ≤1.0 | ≤2.0 | 12-15 | 22-24 | - | 950 ° | 耐長(zhǎng)時(shí)間高溫 |
310S | ≤0.08 | ≤1.5 | ≤2.0 | 19-22 | 24-26 | - | (國(guó)產(chǎn))1000 ° (進(jìn)口)1150 ° | 耐高溫及高溫拉伸 |
314 | ≤0.25 | ≤1.5-3.0 | ≤2.0 | 19-22 | 23-26 | - | (國(guó)產(chǎn))1050 ° (進(jìn)口)1250 ° | 在310基礎(chǔ)上提高抗氧性 |
CI20NI80 | ≤0.15 | ≤0.4-1.3 | ≤0.7 | 75-78 | 20-23 | - | 1200 ° | 耐高溫、抗氧化 |